Components at user site after the floor life has expired or other conditions have occurred which indicate excess moisture exposure are to be re-baked / drying to reset the floor life clock.

 

Rebaking could be done per customer’s specification or otherwise per JEDEC Standard J-STD-033.

 

Dry pack / vacuum seal is being done within 2 hours after components are out from the oven.